Geotextiles

SC 2000 Woven Geotextile

Test

 

 

Tensile strength (kN/m)

Warp
Weft

12
12

Tensile strength at 50% extension (kN/m)

Warp
Weft

25
15

CBR push-through resistance (N)

 

1800

Cone drop penetration (mm)

 

14

Apparent opening size (µm)

 

150

Waterfl ow normal to plane (l/m2/sec)

 

22

Weight (g/m2)

 

95

Roll width (m)

 

45

Roll length (m)

 

100

All figures are the mean of several tests to the relevant British Standard Methods of Test for Geotextiles

Axtex Highflow Geotextile

Test

Standard

 

WHF

Tensile strength (kN/m)

EN 10319

Warp
Weft

27
16

Elongation at max. load (%)

EN 10319

Warp
Weft

28
14

CBR puncture resistance (N)

EN ISO 12236

-

2000

Cone drop penetration (mm)

EN 918

-

14

Pore size 90% fi ner than (microns)

EN ISO 12956

-

380

Water permeability (m/sec)

EN ISO 11058

-

75 x 10

Effect of UV light

 

The polypropylene used contains a UV inhibitor

Weight (g/m2)

   

120

Roll size

Width

 

4.5

 

Length

 

100

All figures are the mean of several tests to the relevant British Standard Methods of Test for Geotextiles

PLEASE NOTE: Geotextiles should be lapped by a minimum of 300mm during installation.